The general process of PEEK injection molding is as follows:
1. Drying: The particulate polymer generally absorbs 0.5% w/w of atmospheric moisture. For best results, it should be dried until the moisture is less than 0.02% w/w. The material can be placed in an air circulating oven, dried at least at 150 ° C for 3 hours, or dried at 160 ° C for 2 hours. If it is dried in a dry box, the thickness of the raw material in the tray should not exceed 25 mm and prevent contamination.
2. Recycling: The remaining material can be recycled and injected into pure materials. It is recommended that the recycled material without filler should not exceed 30% of the total weight, and the recycled mixture containing the filling should not exceed 10% of the total weight.
3. Thermal stability: If the equipment is shut down during the melting process and the polymer residence time does not exceed 1 hour, there is no significant degradation of the material at a temperature of 360 °C. However, if the downtime exceeds 1 hour, the temperature of the cylinder should be reduced to 340 °C. At this temperature, the material can be kept stable for several hours. When the processing is continued, the temperature of the cylinder must be increased. If the downtime is more than 3 hours, The cartridge should be cleaned. Materials which are stable at 380 ° C, such as polyether sulfone or polyetherimide, can also be cleaned with low MFI polyethylene.
4. Injection machine: The melting point of the polymer is 343 ° C, which can be applied to traditional machines that can keep the melt temperature at 360-400 ° C.
5. Cartridge capacity: Due to the high processing temperature of the PEEK polymer, the residence time of the material must be as short as possible. The ideal barrel capacity is 2-5 times the total shot weight.
6. Nozzle and latching system: The melting point of the polymer is very high. If the temperature drops below 343 °C, the melt will solidify very quickly. Therefore, it is necessary to install a heater large enough at the nozzle to prevent the "cooling of the injection molding" from being caused by the cooling.
7. Screw: It is recommended that the minimum length-to-diameter ratio L/D of the screw is 16:1, but the L/D ratio between 18:1 and 24:1 should be preferred.
8. Barrel temperature: The unreinforced level is 360-380 ° C, and the enhanced level is 380-400 ° C.
9. Mold temperature: The surface temperature of the mold is 175-205 °C.
10. Injection pressure: The general injection pressure is 70-140 MPa.
11. Injection speed: medium to high speed.
12. Back pressure: It is recommended that the back pressure be set to 0-1.0 MPa (0-10 kgf/cm2).
13. Screw speed: The general screw speed is 50-100 rpm. For the reinforcement level, it is recommended to use a lower screw speed.
14. Mold shrinkage: Different grades of polymer have different shrinkage rates, the unfilled grade is about 1.2-2.4%, and the fill grade is: 0.1-1.1%.
15. Secondary processing: secondary processing such as bonding, tapping, press-in, metal inserts, cutting and surface metallization.
Bizimle iletişime geçin

Author:

Ms. He Lichun

Phone/WhatsApp:

+8613906114773

Popüler Ürünler
Şirket haberleri
You may also like
Related Categories

Bu tedarikçi için e-posta

Konu:
E-posta:
İleti:

Your message must be betwwen 20-8000 characters

Bizimle iletişime geçin

Author:

Ms. He Lichun

Phone/WhatsApp:

+8613906114773

Popüler Ürünler
Şirket haberleri

Ev

Product

Phone

Hakkımızda

Sorgulama

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Gönder